File Type | Title |
---|---|
![]() | REDCOR® steel - Weathering steel (plate) AS/NZS 3678 – WR350L0B MOD 400, WR350L0Z35B MOD 400 Datasheet Low phosphorous structural weathering steel with nominal yield strength of 400MPa for thicknesses from 10 to 70mm with guaranteed impact performance and an option for improved through-thickness ductility (z test). |
![]() | REDCOR® weathering steel (coil) AS/NZS 1594 - HW350A Datasheet High phosphorous structural weathering steel with a minimum yield strength of 340MPa. |
![]() | REDCOR® weathering steel (coilplate) AS/NZS 1594 - HW350A Datasheet High phosphorous structural weathering steel with a minimum yield strength of 340MPa. |
![]() | REDCOR® weathering steel AS/NZS 1595 - CW300A Datasheet High phosphorous structural weathering steel with a minimum yield strength of 300MPa. |
![]() | REDCOR® weathering steel AS/NZS 3678 - WR350A, WR350L0A Datasheet High phosphorous structural weathering steel with nominal yield strength of 340MPa for thicknesses from 8 to 12mm with an option for guaranteed impact performance at 0°C. |
![]() | REDCOR® weathering steel AS/NZS 3678 - WR350B, WR350L0B, WR350L20B Datasheet Low phosphorous structural weathering steel with nominal yield strength of 340MPa for thicknesses from 10 to 80mm with options for guaranteed impact performance at 0 and -20°C. |
![]() | REDCOR® weathering steel AS/NZS 3678 - WR350Z25B, WR350L0Z25B Datasheet Low phosphorous structural weathering steel with nominal yield strength of 340MPa for thicknesses from 10 to 80mm with improved throughthickness ductility (z test) and an option for guaranteed impact performance at 0°C. |
![]() | REDCOR® weathering steel AS/NZS 3678 - WR350Z35B, WR350L0Z35B Datasheet Low phosphorous structural weathering steel with nominal yield strength of 340MPa for thicknesses from 10 to 80mm with improved throughthickness ductility (z test) and an option for guaranteed impact performance at 0°C. |